求翻译:It is good practice to mechanically clean and degrease the joint surface before applying flux. Heat slowly and evenly to the brazing temperature, without local overheating. Use the flux as a temperature guide - it will become clear or opaque as brazing temperature is approached. If blackening of the flux occurs this is是什么意思?![]() ![]() It is good practice to mechanically clean and degrease the joint surface before applying flux. Heat slowly and evenly to the brazing temperature, without local overheating. Use the flux as a temperature guide - it will become clear or opaque as brazing temperature is approached. If blackening of the flux occurs this is
问题补充: |
|
2013-05-23 12:21:38
机械清理和脱脂申请前通量的关节面,它是很好的做法。热钎焊温度缓慢而均匀,无局部过热。使用温度指南通量 - 它会变得清晰或不透明的钎焊温度接近。如果发黑的光通量发生,这往往是通量不足,过热或磁通疲惫的迹象。
|
|
2013-05-23 12:23:18
这是很好的做法,机械地清洁和除油干燥器联合表面的申请前通量。 热缓慢和均匀的钎焊温度,没有当地过热。 使用的通量的温度指南-它将成为明确或不透明的钎焊温度是接触。 如果涂炭生灵的通量发生这常常是不足通量的迹象,过热或通量用尽。
|
|
2013-05-23 12:24:58
|
|
2013-05-23 12:26:38
它是机械地清洁和通量在应用之前脱脂关节面很好的做法。无局部过热钎焊温度,热慢慢地、 均匀。使用通%E
|
|
2013-05-23 12:28:18
|